Tile Adhesive Diamond

TIGONIS Diamond PU is a two part modified Polyurethane multipurpose thin-set adhesive for fixing all type of tiles and stones including (Composites engineered stone) on interior and exterior surface like Concrete Masonry & Brick Masonry, Cement mortar Beds & Plaster, Metal Substrates, dry wall boards, plywood ,all types of wood Substrate. It has been designed for fixing water Sensitive tiles/ stones on deformable or absorbent/ non-absorbent Substrate. It is highly flexible and water freeze and thermal shock resistant when fully cured.

General Details

Modified polyurethane based multipurpose adhesive for stone & tile fixing

Physical Properties
Appearance PART.A: White Paste                     

PART.B: Cream Paste

Mixed Density 1.65 ± 0.1 kg / Liter
Shelf Life 12 Month in the Original Packing
Mixed Material Appearance Off White Paste
Open Time Minimum 60 minute
Adjustability Minimum 60 minute
Pot Life Minimum 60 minute
Vertical Slip  ≤ 0.5 mm
Foot Traffic = 24 Hour
Grouting = 12 Hours on walls

= 24 Hour on floors

Temperature range for application 10 to 40
Coverage 20-25 sqft per 4 kg Bucket

 

Performance As per EN12004 (R2T)

Requirement Test Result
Initial Shear Adhesion Strength ≥ 2.0 N/mm2 ≥ 5.0 N/mm2
Shear Adhesion Strength after water immersion ≥ 2.0 N/mm2 ≥ 5.0 N/mm2
Shear Adhesion Strength after  thermal shock ≥ 2.0 N/mm2 ≥ 5.0 N/mm2
Slip resistance ≤ 5.0 N/mm ≤ 0.3mm

 

Performance As per IS 15477:2019 ( Type 5 T S2)

Requirement Test Result
Tensile Adhesion at Dry Condition at 28 days ≥ 2.0 N/mm2 ≥ 2.0 N/mm2
Tensile Adhesion at Wet Condition           – ≥ 1.5 N/mm2
Shear Adhesion at Dry Condition ≥ 6.0 N/mm2 ≥ 7.0 N/mm2
Shear Adhesion at  Wet Condition             – ≥ 5.0 N/mm2
Shear Adhesion at Heat Ageirg ≥ 3.0 N/mm2 ≥ 5.0 N/mm2
Deformability (s2) ≤ 5mm ≤ 30mm

NOTE: Test results are indicative as per testing method specified in standard. Test results may vary as per substrate. Site condition & testing machine etc. Actual  held performance will depend on installation method and site conditions.

Packaging

4 Kg Bucket (PART A : 3.200 Kg/ PART B : 0.800 Kg)

 

Mixing

Tigonis Diamond Adhesive is prepared by mixing together parts A and part B from the bottom upwards, using a low-rev (=400/ min) halicidalagitator with present mixing of 4:1 of the packs. Pour Part B into the bucket containing Part- A, being careful to mix the two parts uniformly until a smooth paste is obtained.